ENCO 1/7/2016
毛坯的表面要求
毛坯-Raw finish
焊道要顺畅-the welding bead must be smoothly
无凹陷-no dents
无针孔-No pin holes
焊道无裂痕- No cracks on welding bead
管材未变形- No deformed tubing
导线座未变形- No deformed cable guide
表面无磕伤- No scratches on the surface
尺寸要合图- Follow the drawing dimensions
烤漆的基本要求
Painted finish
无色差- No deviation
无灰尘无沙粒- No dusty , No sandy
无凹陷-no dents
无麻面,无橘皮- No orange peel
无划伤- No scratches
无精油聚垂- No drops
头管中管五通要防漆- No painting inside the HT ST BB
无污染- No pollution
烤漆检测方法
Cross cut 百格测试
Ball drop 落球实验(1.5米高,铁球直径12.7mm )
贴花的基本要求
Applying the decal
贴花图案必须与客人的设计图稿100%一致- follow the artwork design 贴花位置必须与稿件位置一致- follow the artwork design
贴花无破损- No broken decals
贴花无褶皱,无翘边- No wrinkles on the decal
贴花无气泡- No bubbles under the decal
无漏标- No missing decal
贴花无歪斜- no deflection
贴花无颠倒- no reversion
Checking zones 检查区域
Zone A Zone B Zone C
ENCO 1/7/2016
毛坯的表面要求
毛坯-Raw finish
焊道要顺畅-the welding bead must be smoothly
无凹陷-no dents
无针孔-No pin holes
焊道无裂痕- No cracks on welding bead
管材未变形- No deformed tubing
导线座未变形- No deformed cable guide
表面无磕伤- No scratches on the surface
尺寸要合图- Follow the drawing dimensions
烤漆的基本要求
Painted finish
无色差- No deviation
无灰尘无沙粒- No dusty , No sandy
无凹陷-no dents
无麻面,无橘皮- No orange peel
无划伤- No scratches
无精油聚垂- No drops
头管中管五通要防漆- No painting inside the HT ST BB
无污染- No pollution
烤漆检测方法
Cross cut 百格测试
Ball drop 落球实验(1.5米高,铁球直径12.7mm )
贴花的基本要求
Applying the decal
贴花图案必须与客人的设计图稿100%一致- follow the artwork design 贴花位置必须与稿件位置一致- follow the artwork design
贴花无破损- No broken decals
贴花无褶皱,无翘边- No wrinkles on the decal
贴花无气泡- No bubbles under the decal
无漏标- No missing decal
贴花无歪斜- no deflection
贴花无颠倒- no reversion
Checking zones 检查区域
Zone A Zone B Zone C